Molybdenum Metal Briquettes
Processed by pressing and sintering Molybdenum-metal powder.
Common uses: Alloy component in foundries and steel industry. Produced in following facility: Chemiemetall Chemical Specifications
(*)Excluding gas content. Physical Properties
Further elements and specifications upon request. Packaging Options
Other packaging upon request. Handling instructionsWhen handling the material the working instructions valid in each country must be adhered to. |